Evaluation of conditions for hydrogen induced degradation of zirconium alloys during fuel operation and storage

International Atomic Energy Agency

Pocket

309:-

Funktionen begränsas av dina webbläsarinställningar (t.ex. privat läge).

Tillfälligt slut online – klicka på "Bevaka" för att få ett mejl så fort varan går att köpa igen.

  • 79 sidor
  • 2016
This publication reports on the work carried out in 2011-2015 in the coordinated research project (CRP) on the evaluation of conditions for hydrogen induced degradation of zirconium alloys during fuel operation and storage. The CRP was carried out to evaluate the threshold condition for delayed hydride cracking (KIH) in pressurised water reactors and zircaloy-4 and E635M fuel claddings, with application to in-pile operation and spent fuel storage. The project consisted of adding hydrogen to samples of cladding and measuring KIH by one of four methods.
  • Författare: International Atomic Energy Agency
  • Format: Pocket/Paperback
  • ISBN: 9789201107152
  • Språk: Engelska
  • Antal sidor: 79
  • Utgivningsdatum: 2016-01-20
  • Förlag: IAEA